IllustrationThe right board depends on where it sits and what holds it, so a single board type across a hotel project is always wrong somewhere.
In short
- Use plywood wherever a hinge, a runner or moisture is involved; particleboard loses screw grip fast.
- Particleboard swells 8 to 12 percent after a 24 hour soak, moisture resistant plywood only 1 to 3.
- Verify board type by weight and by the cut edge, and check moisture content sits at 8 to 12 percent.
Three boards do most of the work in hotel furniture: particleboard, medium density fibreboard and plywood. They differ in density, screw holding strength, moisture behaviour and price, and the difference matters in specific places. A factory that uses one board everywhere is saving its own effort, not the project's money.
In short: particleboard for carcasses with faced surfaces, MDF for shaped and painted faces, plywood wherever water or a screw load is involved. Never use particleboard for a bathroom cabinet or a door hinge zone.
How do the three compare on the numbers that matter?
Particleboard runs 650 to 720 kg per cubic metre, MDF 800 to 850, and plywood 9 to 13 plies at similar density but with far better screw holding along the face. Particleboard holds a screw about 800 to 1,200 N on the face, MDF around 1,000 to 1,500, plywood often double that because the load is carried across plies. Thickness swelling after 24 hours of water soak is roughly 8 to 12 percent for particleboard, 5 to 8 for MDF, and 1 to 3 for moisture resistant plywood.
Where does each board belong?
Particleboard: wardrobe and nightstand carcasses with a faced surface on both sides, where cost matters and the board never sees water. MDF: door faces, headboard panels, moulded and painted profiles, because it machines to a clean edge and takes a smooth lacquer. Plywood: bathroom vanities, kitchen units, any panel carrying a hinge or a heavy drawer runner, and anything on a wall that sees moisture.
Why is the hinge zone the deciding detail?
Because that is where failures start. A 2,100 mm door weighs 12 to 16 kg and hangs on two or three hinges, each applying a pull out force of about 400 N at the panel. Particleboard at 18 mm loses screw grip after two or three adjust cycles and the hinge pulls out, leaving a hole nobody can repair on site. A plywood core, or a particleboard panel with an inserted plywood hinge block, solves it for a few dollars per door.
What about formaldehyde and fire?
Specify E0 for boards inside the guest room and check the emission declaration per board, not per factory. Fire performance depends on the facing and the assembly, so a B1 core is not automatically a class B panel; the complete build has to be tested or declared. Do not accept a certificate for a different thickness from the one you are buying.
How should a buyer verify what arrives?
Weigh a sample. An 18 mm particleboard panel of 600 x 400 mm weighs about 3.3 kg; the same panel in MDF is about 4.1 kg. Check the core at a cut edge: particleboard shows coarse flakes, MDF shows a fine uniform fibre, plywood shows plies. For a plywood panel, count the plies and check there is no void at the centre. And check the moisture content with a meter, which should read 8 to 12 percent, not 15.
What belongs in the material specification? 1. Board type and grade per component. 2. Density range or weight per square metre. 3. Emission class with the standard number. 4. Moisture resistance requirement where relevant. 5. Hinge and runner fixing method, with any insert block. 6. Edge banding and sealing requirement.
The limitation: board grade fixes durability and emissions, not design. Two projects with identical boards can look entirely different, and the cheaper board is not always the one that fails first; poor edge sealing fails before any board choice does.